The most recent test revealed a manufacturing error in the length of the phenolic liner. This resulted at a burnthrough near the forward closure.

Test #DateSiteResult
XB-98-4G #1 Crow IslandUndetected stress concentrator in nozzle lead to a cracked nozzle.
XB-98-4G #2 Crow IslandPoor sealing on thermal liner lead to runaway burn-through
XB-98-4G #39-23-2017Crow IslandFull Duration

 