 5-Layer Fiberglass10-Layer Fiberglass
Control (West Systems epoxy)  
West Systems + Phenolic microballoons  
West Systems + Cork microballoons  
West Systems + High temperature paint  
West Systems + Cotronics 4700  

Sample Preparation:

  1. Used West Systems epoxy to make 4 of 8" x 8" sheets of fiberglass (2 x 5 layers, 2 x 10 layers)
  2. Sand with a Dremel, then with 400-grit sandpaper. Make sure to sand the shiny side
  3. Mark and cut into 1.5" x 1.5" squares.
  4. Record mass of each sample.

Below is the test matrix for the parameters measured during this test. (Fill later with results).

...